SteveD wrote:Here's a response re: the short term look ...from George Strong in the UK. bmbikes forum.
Barrel fins seem OK with the silver leaf rub'n'buff even after prolonged heat - doesn't look any different after about 500 miles. Same with base of barrel and crankcase ... I'm still on the first tube after covering everything alloy, with a spare on the shelf.
Unfortunately, that doesn't tell us anything about the higher heat application of the heads. Course, if jj tries it, they we can ALL find out!